API 5L X46 ERW Pipe
API 5L X46 Psl1 High Yield Tube, we provide high-quality steel pipes to customers all over the world according to their needs.
API 5L X46 ERW steel Pipes have a steel grade of X46, a quality grade of PSL1, and a production process of electric resistance welding (ERW). The ERW process is suitable for producing larger diameter pipeline pipes. The X46 electric resistance welded pipe body is made of steel plates curled and welded, and then heat treated to meet specific mechanical property requirements.
API standard produced X46 straight seam pipeline steel pipe is mainly used to transport gas and liquid objects such as oil and natural gas.
API 5L X46 Welded Line Pipes PSL2 Chemical Composition
| API 5L X46 PSL2 Pipe | |
| ERW: {{0}}.375″ through 30″ HF: 0.840″ through 24″ DSAW/SAWL: 12.75″ through 144″ SMLS: 0.840″ through 26″ HSAW: 8.625″ through 144″ | |
| ERW: {{0}}.120″ through 1.000″ HF: 0.120″ through 1.000″ DSAW/SAWL: 0.250″ through 6.000″ SMLS: 0.250″ through 2.500″ HSAW: 0.250″ through 1.000″ | |
| Single Random Double Random Custom (up to 300′) |
Mechanical Properties of API 5L X46 Welded Steel Pipes PSL2
| API 5L X46 | (PSL2) |
|---|---|
| 46,400 psi | |
| 76,100 psi | |
| 63,100 psi | |
| 110,200 psi |
API 5L X46 ERW Carbon Steel tube

gnee has 14 steel production lines, 10 processing equipment for processing, bending, painting, heat treatment, cutting, drilling, beveling, tempering, surface treatment, complete testing equipment and strong technical force. The annual production capacity is more than 60,000 tons.

Популярни тагове: api 5l x46 erw pipe, China api 5l x46 erw pipe manufacturers, suppliers, factory, Военна тръбаСплав 20 тръбаПоцинкована стоманаAPI 5L линейна тръба за транспортиране на гориво